O/W-Sonnenschutzcreme / Sun protection cream O/W
Rezeptur Nr./Formulation no. : 92/313/2 LSF / SPF 10-15 (DIN/calculated)
Bestandteil/Component % Funktion/Function
I.
Emulgade® SE
Glyceryl Stearate (and) Ceteareth-20 (and) Ceteareth-12 (and) Cetearyl Alcohol (and) Cetyl Palmitate

6,0 O/W-Emulsionsgrundlage SE/ O/W emulsion base SE
Cetiol® LC
Coco Caprylate/Caprate

3,0 Emollient
Cetiol® SN
Cetearyl Isononanoate

3,0 Emollient
Cetiol® SB 45
Butyrospermum Parkii

2,0 Emollient
Copherol® 1250
Tocopheryl Acetate

1,0 Wirkstoff/active ingredient
Parsol MCX (Givaudan)
Octyl Methoxycinnamate

7,5 UV-Filter
Parsol 1789 (Givaudan)
Butyl Methoxybenzoylmetha
ne

2,5 UV-Filter
Uvinul M 40 (BASF)
Benzophenone-11

1,0 UV-Filter
II.
Glycerin 86%

3,0 Moisturiser
Aqua

55,62  
III.

Carbopol 980 (Goodrich)
(2%ige Quellung/2% swelling

15,0 Stabilisator/stabiliser
IV.
KOH 20%

0,18 Neutralisationsmittel/neutraliser
V.

Hydagen® B
Bisabolol

0,2 Wirkstoff/active ingredient
Konservierungsmittel/preservative

n.B./q.s.  

Viskosität/viscosity mPas Brookfield, RVF, 23� C, Spindel/ rotor: Helipath TE UpM/Rpm: 4

132.000

 
 

Herstellung im Labormaßstab

1. Komponenten unter I. bei 80 - 85�C schmelzen und homogen vermischen.
2. Komponenten unter II. ebenfalls auf 80 - 85� C erwärmen und unter Rühren/Homogenisieren zu Phase I. geben. 5 Minuten bei Temperatur rühren.
3. Unter weiterem Rühren und Luftkühlung so abkühlen, daß die Emulsion in ständiger homogener Bewegung bleibt und keine Luft eingerührt wird. Bei 65 - 55� C zur Struktur- sowie Stabilitätsverbesserung mit geeignetem Dispergierkopf homogenisieren (z. B. Ultra Turrax).
4. Bei 50�C Zugabe der Carbopolquellung,homogen rühren.Neutralisation mit Phase IV und auf 30�C abkühlen.Zugabe Phase V.

Preparation in the laboratory

1. Melt the components listed under I at 80 - 85�C and stir until homogeneously.
2. Heat the components listed under II to 80 - 85�C and add to phase I while stirring. Stir for 5 minutes at this temperature.
3. Allow the emulsion to cool with stirring in such a way that it remains in continual motion. Avoid the incorporation of air.
Homogenise at 65-55�C by means of a suitable dispersion unit(e.g.Ultra Turrax)in order to improve both stability and structure.
< 4. Add Carbopol swelling at 50� C. Stir until homogeneous. Neutralize with phase IV and allow to cool to 30�C. Add phase V.


All products in the text marked with an ® are registered trademarks of the HENKEL group.

Suggestions for processing and use of our products as well as possible formulation suggestions are provided noncommittally in accordance with our knowledge and information. They do not discharge our customers from testing the products on suitability for processes and purposes they are destined for. We are only liable for a damage caused intentionally or by gross negligence. However, we are under no circumstances liable for consequential damage. Each processor is liable for the compliance of all legal regulations, including patent legislation.

Henkel does not guarantee the suitability of a product for a user-specific purpose.

H E N K E L  K G a A Care Chemicals Division Düsseldorf